MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 06396 Adhesion Promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: 3M Adhesion Promoter 06396 is a liquid primer used to improve the adhesion of 3M Automotive Attachment Tapes to most low surface energy plastic materials as well as injection-molded body side moldings and claddings used for automotive exterior trims. This world include common low surface energy plastics used for automotive interior and exterior trim applications (TPO, PPO, PP, PC, PC+ABS, etc). Since formulations and surface energies can vary for these types of materials, each application should be verified through testing. 3M adhesion promoter 06396 is specifically formulated to be used on plastic parts with 3M Acrylic Foam Tapes and 3M Acrylic Plus Tapes (3M part numbers 06377, 06378, 06380, 06381, 06382, 06383, 06385, 06386 and 06397) for automotive applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.815 g/cc0.0294 lb/in³
Solids Content 5.0 %5.0 %
Viscosity 25 cP25 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point -20.0 °C-4.00 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 4.00 - 38.0 °C
12.0 Month
@Temperature 39.2 - 100 °F
 
Descriptive Properties
AppearanceStraw

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35421 / 170168

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.