MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Armohib CI-209 Imidazoline
Categories: Other Engineering Material

Material Notes: Cationic imidazoline oil-based mud additive in a liquid solution with a pH of 11.

Applications: Armohib CI-209 is a complex amidoamine. Corrosion inhibitors formulated with this unique organic base display high film persistency against the attack of severely corrosive fluids and gases in sour (H2S) and sweet (CO2) environments. Because the product can be formulated into oil-soluble, oil-soluble/water-dispersible or water-soluble inhibitors, the finished formulations readily disperse in hydrocarbon solvents, water and brine. As a result, corrosion inhibitors formulated with Armohib CI-209 are able to work effectively in a wide range of tough chemical and physical environments, providing the formulator with superior versatility and low inventory requirements.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³
pH 10 - 1210 - 125% in 3:1 IPA/H20
Brookfield Viscosity 200 cP200 cP
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -11.0 °C<= 12.2 °F
Flash Point >= 93.3 °C>= 200 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.20 %<= 0.20 %
 
Descriptive Properties
Amine number4.5-4.8 meq/g
AppearanceGreen amber liquid
OdorAmine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY245 / 285768

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.