MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Cristal™ One Pro MR Renew-30 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ One Pro MR Renew-30 is a copolyester that contains mold release for ease of injection. It is designed to be fully compatible with the PET recycling stream. It enables recyclable cosmetics packaging that is tough, exhibits good chemical resistance. It is suitable for molding thick-walled transparent containers or parts (up to approximatively 12mm), while maintaining clarity and color. Cristal™ One Pro MR Renew-30 meets the definition of resin identification code #1 (RIC1) as defined by the California Assembly Bill (#906) and by ASTM D7611, Association of Plastic Recyclers (APR) as well as European PET Bottle Platform (EPBP). Other end-product attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC-certified recycled content by mass balance allocation.

Applications

  • Bottles-color cosmetics pkg
  • Bottles-skin care pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Ability to mold thick parts
  • Excellent processing capabilities
  • Good chemical resistance
  • Good gate aesthetics
  • Good toughness
  • Recyclable with the PET stream
  • Transparency

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 54.0 MPaASTM D638
Elongation at Break >= 150 %ASTM D638
Tensile Modulus 2300 MPaASTM D638
Flexural Yield Strength 78.0 MPaASTM D790
Flexural Modulus 2400 MPaASTM D790
Izod Impact, Notched 52.0 J/mASTM D4812
Izod Impact, Unnotched NBASTM D4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 280 °C
Mold Temperature 16.0 - 38.0 °C
Drying Temperature 130 - 140 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4044 / 323667

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.