MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation Bisco® A2 R 3.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tear strength obtained from the embedded fiberglass. I
A2 is light gray in color.

Applications:

  • Aircraft acoustic insulation
  • Noise reduction liner for interior panels
  • Aircraft flooring noise barrier
  • Rail Interior noise blocker

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60without reinforcement; ISO 7619
Tensile Strength 8.00 MPafill; ISO 37 Type 2
 12.0 MPawrap; ISO 37 Type 2
Tear Strength 10.0 kN/mISO 4674-1 Method B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -50.0 °C
 
Descriptive Properties
Areal density0.3 g/cm²ISO 2286-2
Flammability TestPassFAR 25.853a and FAR 25.856 (a) (AITM 2.0053)
Polymer Typewrap/fill
Smoke Density (min)Passes smoke gas components test AITM 3.0005FAR 25.853 (a-1) (AITM 2.0007)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROGA909 / 138349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.