Notes: Monprene IN-22946DV XRD2 is a high performance thermoplastic elastomer vulcanizate used in industrial applications. Monprene IN-22946DV XRD2 is a low density, high hardness, RoHS compliant exhibiting excellent UV absorbing characteristics. This grade can be processed by extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Abrasion Resistant; Filled; Good Melt Strength; Good Processability; Good Processing Stability; High Hardness; Light Stabilized; Low Flow; Low Density; Low Specific Gravity; Lubricated; Slip; UV Absorbing Uses: Capstock; Gaskets; Glazing; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weather-stripping RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |