MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Freudenberg N470 Nitrile Elastomer (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: CHEMIGUM® , HYCAR® , PARACRIL® , PERBUNAN®, KRYNAC®, NYSYSN®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Original Property; ASTM D2240
 67ASTM Reference Fuel B Immersion, 168 hours; ASTM D2240
 71ASTM IRM-903 Oil Immersion, 70 hours; ASTM D2240
 77Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 17.8 MPaOriginal Property; ASTM D1414
 1320 psiASTM Reference Fuel B Immersion, 168 hours; ASTM D1414
 2614 psiAir Aging, 70 hours; ASTM D1414
Elongation at Break 377 %Original Property; ASTM D1414
 267.67 %ASTM Reference Fuel B Immersion, 168 hours; ASTM D1414
 324.22 %Air Aging, 70 hours; ASTM D1414
Compression Set 64 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395 Method B
 
Descriptive Properties
Bend (flat)PassAMS 7270K
Bend OvalPASSLow Temp. Brittleness, Fuel B, 48 hours at 23°C, then Fuel A, 48 hours at 23°C, then Fuel A 5 hours at -40°C per AMS-7270K paragraph 4.5.2
Volume Change (%), ASTM D471-1.4Low Temp. Brittleness, Fuel B, 48 hours at 23°C, then Fuel A, 48 hours at 23°C, then Fuel A 5 hours at -40°C per AMS-7270K paragraph 4.5.2
 15ASTM IRM-903 Oil Immersion, 70 hours
 34ASTM Reference Fuel B Immersion, 168 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Freudenberg N470 Hydrocarbon Elastomer Nitrile
Freudenberg N442 Nitrile Elastomer (NBR)
Freudenberg N431 Nitrile Elastomer (NBR)
Freudenberg N475 Nitrile Elastomer (NBR)
Freudenberg N445 Nitrile Elastomer (NBR)

PSIMR141 / 79103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.