Desmoderm VP LS 2262 is a one-component polyether urethane based on an aromatic diisocyanate. Uses: Desmoderm VP LS 2262 is used as the hard component in the coagulation process. It retains its good property profile only in combination with similarly structured urethane (Desmoderm 43195 Granular). Desmoderm VP LS 2262 is suitable for use in the manufacture of materials for clothing, shoe uppers, bags/luggage and athletic shoes as well as upholstery. Information provided by Covestro |