MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Redwood Plastics Redco™ X-STATIC UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Redco™ X-Static eliminates static electricity hazards common in bulk material applications. Redco™ X-Static is a special combination of virgin UHMW compounded with Carbon Black to provide anti-static properties while retaining corrosion and wear resistance, low surface friction and high impact strength.

Standard Color: Black

Typical Applications: Bulk material liners, wear strip, chute, bin, hopper, and silo liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 - 0.940 g/cc0.0336 - 0.0340 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 67 - 7067 - 70ASTM D 2240
Tensile Strength 33.0 - 39.0 MPa4790 - 5660 psi2 in./min; ASTM D 638
Tensile Strength, Yield 19.0 - 22.0 MPa2760 - 3190 psi2 in./min; ASTM D 638
Elongation at Break 300 - 400 %300 - 400 %2 in./min; ASTM D 638
Tensile Modulus 0.689 - 1.083 GPa99.9 - 157.1 ksi2 in./min; ASTM D 638
Flexural Modulus 0.689 - 1.033 GPa99.9 - 149.8 ksiASTM D 790
Izod Impact, Notched (ISO) NBNBASTM D 256A
Coefficient of Friction, Dynamic 0.12 - 0.160.12 - 0.16Against Cr-Plated Steel; ASTM D 1894
Coefficient of Friction, Static 0.20 - 0.250.20 - 0.25Against Cr-Plated Steel; ASTM D 1894
Abrasion 1010Sand Slurry, Index (Relative To Steel At 100)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+7 ohm-cm>= 1.00e+7 ohm-cmASTM D 257
Surface Resistance 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C10.0 µin/in-°FASTM D 696

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW002 / 296568

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.