Description: MTM22S is a 140°F (284°F) curing, styrene free, polyester resin matrix offering flexible processing and handling characteristics. MTM22S has been developed specifically for tube rolling applications and can be processed by oven or press molding. Features & Benefits: - Styrene-free
- 60 days out life at 21°C (70°F)
- 12 months storage at -18°C (0°F)
- 100 to 140°C (212 to 284°F) cure temperature
- Oven or press molding
Product Variants: MTM22SB: black pigmented MTM22SG: Green pigmentedNote 1: Material: MTM22S/430 g/m2 8H E-glass unidirectional tape; Cure cycle: 1 hr at 120°C (248°F), 6.2 bar (90 psi) Information provided by Cytec, subsequently acquired by Solvay. |