MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Foster Tear Resistant ProFlex™ 35A SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: ProFlex™ is a comprehensive range of Styrene Ethylene Butylene Styrene (SEBS) Thermoplastic Elastomers (TPEs). These unique polymers offer excellent elastomeric properties, with design flexibility and ease of processing via injection molding and extrusion. ProFlex™ SEBS is available in standard, tear resistant, and ProPell™ formulations across a range of durometers. Foster can also customize formulations if the application requires it. ProFlex™ SEBS was designed to be used in a variety of medical applications including catheters, surgical handles and ergonomic grips. ProFlex™ SEBS is available in a variety of development quantities upon request.

Information provided by Foster Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535ASTM D2240
Tensile Strength at Break 5.21 MPa755 psiASTM D412
Tensile Strength 1.08 MPa
@Strain 100 %
157 psi
@Strain 100 %
ASTM D412
Elongation at Break 640 %640 %ASTM D412
Tensile Modulus 0.00143 GPa0.208 ksiASTM D638
Coefficient of Friction 3.423.42Stainless Steel; ASTM D1894
Tear Strength 13.57 kN/m77.43 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 171 °C320 - 340 °FInjection
 160 - 171 °C320 - 340 °FExtrusion
Middle Barrel Temperature 171 - 182 °C340 - 360 °FInjection
 171 - 182 °C340 - 360 °FExtrusion
Front Barrel Temperature 188 - 199 °C370 - 390 °FInjection
 188 - 199 °C370 - 390 °FExtrusion
Nozzle Temperature 188 - 193 °C370 - 380 °FInjection
Die Temperature 188 - 193 °C370 - 380 °FExtrusion
Mold Temperature 23.9 - 51.7 °C75.0 - 125 °FInjection
Screw Speed 25 - 75 rpm25 - 75 rpmInjection
 50 - 100 rpm50 - 100 rpmExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFOSTER003 / 312442

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.