RTP 200 FR NH is designed for full compliance to both global reglatory and ecolabel restrictions, while offering V-0 performance at a low specific gravity and cost. The halogen-free nature of this material provides very low corrosivity to equipment as well as low smoke toxicity combustion characteristics. |