MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik BREAK-THRU® S 278 Surfactants
Categories: Fluid

Material Notes: Product description: BREAK-THRU® S 278 is a polyether trisiloxane. In aqueous solutions, it shows super spreading and does dramatically reduce surface tension. There-fore, the biological performance of crop protection products can be significantly enhanced by
  • superior wetting of the plant, especially leaves
  • better uptake through cuticular penetration and
  • stomatal flooding.
Application: BREAK-THRU® S 278 can be used in tank mix applications. For tank-mixtures, pesticide manufacturers may suggest a rate of a non-ionic surfactant to be used with their product. Follow the corresponding label recommendation. However, if the pesticide label does not have a specific recommendation for adjuvant use, but does not prohibit its application, BREAK-THRU® S 278 should be applied at rates listed here. Careful observation of spray performance in a trial application with the tank mixture to be sprayed is advised to determine proper and efficient surfactant rates.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Viscosity 10 - 25 cP10 - 25 cP
Surface Tension 21 dynes/cm21 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Pour Point 5.00 °C41.0 °F
Flash Point >= 100 °C>= 212 °F
 
Descriptive Properties
AppearanceColorless to pale straw liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL709 / 196913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.