MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Insulation TRYMER® 2500 Polyisocyanurate Insulation
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: TRYMER™ 2500 insulation is a modified polyisocyanurate cellular material supplied in the form of bunstock for fabrication into sheets, pipe, tank and vessel covering and other shapes for a variety of thermal insulation applications. Although similar in physical form to polyurethane insulations, TRYMER™ 2500 has better dimensional stability over a wider range of temperatures. TRYMER™ 2500 has been specifically formulated to provide excellent thermal insulation properties without the use of CFC or HCFC blowing agents.

Applications: TRYMER™ 2500 is used extensively in industrial and commercial applications within the service temperature range of -297°F to +300°F (-183°C to +149°C). Because of the critical technical design aspects of many of these applications, qualified designers or consultants should design the total system. Some typical applications include:

  • Pipe, tank and vessel insulation
  • Fabricated pipe fitting insulation
  • Core material for architectural and structural panels
  • Insulation for shipping containers, trucks or rail cars
  • Core material for factory built panelized constructions
  • Flat or tapered boardstock for roof insulation

Information provided by ITW Insulation Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0400 g/cc0.00145 lb/in³ASTM D1622
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
immersion; ASTM C272
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.172 MPa25.0 psiPerpendicular to rise-width; ASTM D1623
 0.221 MPa32.0 psiPerpendicular to rise-length; ASTM D1623
 0.241 MPa35.0 psiParallel to rise-thickness; ASTM D1623
Tensile Modulus 0.00500 GPa0.725 ksiPerpendicular to rise-width; ASTM D1623
 0.00621 GPa0.900 ksiParallel to rise-thickness; ASTM D1623
 0.00752 GPa1.09 ksiPerpendicular to rise-length; ASTM D1623
Flexural Strength 0.290 MPa42.0 psiparallel to rise; ASTM C203
Flexural Modulus 0.00538 GPa0.780 ksiparallel to rise; ASTM C203
Compressive Strength 0.207 MPa30.0 psiPerpendicular to rise-width; ASTM D1621
 0.269 MPa39.0 psiParallel to rise-thickness; ASTM D1621
 0.276 MPa40.0 psiPerpendicular to rise-length; ASTM D1621
Compressive Modulus 0.00338 GPa0.490 ksiPerpendicular to rise-width; ASTM D1621
 0.00545 GPa0.790 ksiParallel to rise-thickness; ASTM D1621
 0.00689 GPa1.00 ksiPerpendicular to rise-length; ASTM D1621
Shear Modulus 1.97 GPa285 ksiparallel to perpendicular, avg; ASTM C273
Shear Strength 0.117 MPa17.0 psiparallel to perpendicular, avg; ASTM C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.141 W/m-K0.979 BTU-in/hr-ft²-°FASTM C518
 0.190 W/m-K1.32 BTU-in/hr-ft²-°FAged 180 days; ASTM C518
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -183 °C-297 °F
Flame Spread Index <= 25
@Thickness 25.4 - 152 mm
<= 25
@Thickness 1.00 - 6.00 in
 
Descriptive Properties
Closed Cell Content95%ASTM D2856
ColorTan
Dimensional Stability+0.1% Changeat -23°C, 7 days, Length, ASTM D2126
 +0.1% Changeat -23°C, 7 days, Volume, ASTM D2126
 +0.4% Changeat 70°C, Length, ASTM D2126
 +0.6% Changeat 70°C, Volume, ASTM D2126
 +1.5% Changeat 70°C, 97% RH, 7 days, Length, ASTM D2126
 +2.6% Changeat 149°C, 7 days, Length, ASTM D2126
 +3% Changeat 70°C, 97% RH, 7 days, Volume, ASTM D2126
 +3.6% Changeat 149°C, 7 days, Volume, ASTM D2126
 -0.1% Changeat -40°C, 7 days, Length, ASTM D2126
 -0.2% Changeat -40°C, 7 days, Volume, ASTM D2126
R-Value0.93 (m²-°C)/Waged 180 days, ASTM C518
 1.25 (m²-°C)/WASTM C518
Surface Burning Characteristics295Smoke Generation
Water Vapor Permeability3 perm-inchASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ITW Insulation TRYMER® 2000 XP Polyisocyanurate Insulation
DIAB Rigid Foam IPN 20-649 Type 1
Anocast Silica-filled Epoxy Polymer Composite
Rogers Arlon Thermabond® T-20 NP (99770W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Rogers Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate

PITWZ011 / 187077

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.