MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meyors Chemical CENWAY CI IR 1301
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Composition: Copolymer rubber of Chlorinated Isobutylene-Isoprene with low Mooney viscosity.

Applications: Chlorobutyl Rubber CI IR 1301 has superior air impermeability, outstanding performance of heat-resistance, chemical corrosion-resistance, thermal aging resistance, and good curing performance. It can be widely used for tire inner liners, medical stoppers, corrosion-resistance lining, protective clothing, shoes production and TPV industry.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 33 - 43
@Temperature 125 °C
33 - 43
@Temperature 257 °F
ML1+8; ISO 289/ASTM D1646
Ash <= 0.70 %<= 0.70 %ISO 247/ASTM D5667
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 1.0 - 1.4 %1.0 - 1.4 %
 
Descriptive Properties
AppearanceOff-white
Content>0.02%Antioxidant (non-staining)
Cure Characteristics0.6-2.1 mints1, Rotorless cur (MDR)
 1.6-3.4 dN-mFL, ISO 6502/ASTM D5289
 1-5 mintc50, 160?×40min, 0.5°arc
 5.2-11.8 mintc90, 160?×40min, 0.5°arc
 6.5-9.5 dN-mFH, ISO 6502/ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMEYORS020 / 316602

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.