Hostacom TRC 787N high melt flow, 1,850 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity, and impact and scratch and mar resistance. It was designed primarily for molded-in color automotive instrument panels. Status: Development Availability: North America Application: Instrument Panels Processing Method: Injection Molding Features: Good Colorability, Good Flow, Low Gloss, High Impact Resistance , Good Moldability , Scratch Resistant, High Stiffness Information provided by LyondellBasell. |