MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Azoty Tarnow™ TARNOFORM 500 HI4 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Easy flow high impact grade, possessing also high damping capacity

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 0.41 %0.41 %23°C/24 hr; ISO 62
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
21 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ISO 2039-2
Ball Indentation Hardness 83.0 MPa12000 psi358 N; ISO 2039-1
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break 32 %32 %ISO 527
Flexural Strength 42.0 MPa6090 psiISO 178
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dissipation Factor 0.034
@Frequency 1e+6 Hz
0.034
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.48 J/g-°C0.354 BTU/lb-°F
Melting Point 164 - 167 °C327 - 333 °F10°C/min.; ISO 3146
Vicat Softening Point 122 °C252 °F50 N; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 210 °C356 - 410 °FBarrel temperature
Mold Temperature 50.0 - 80.0 °C122 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZAK035 / 72874

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.