Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack. Uses: Blown and flat die/cast film extrusion and cable jacketing. Available in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |