MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cookson Group Plaskon® S-7P Epoxy Encapsulant  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Test specimens were transfer molded and post cured 4 hours at 175°C.

A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically formulated to provide a lower viscosity for those low stress applications where wire sweep may be a concern. Excellent low stress properties; Consistent moldability (low viscosity, easy of mold filling, fast cycles and good hot hardness); Outstanding cosmetics and markability; Superior reliability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.82 g/cc0.0658 lb/in³
Viscosity 8500 cP
@Temperature 175 °C
8500 cP
@Temperature 347 °F
Automatic orifice Viscosity
Linear Mold Shrinkage 0.0037 cm/cm0.0037 in/in
Spiral Flow 100 - 130 cm39.4 - 51.2 in177°C/1000 psi
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373
Tensile Strength, Ultimate 62.0 MPa8990 psi
Flexural Strength 103 MPa14900 psi
Flexural Modulus 13.0 GPa1890 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
Dielectric Strength 16.0 kV/mm406 kV/in
Dissipation Factor 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
Arc Resistance 180 sec180 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
10.0 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature 20.0 °C
25.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 150 °C302 °F
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 185 °C338 - 365 °FMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Encapsulant, Unreinforced
Cookson Group Plaskon® S-7S Epoxy Encapsulant

PCOOK326 / 21422

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.