MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta EndurX™ BP11NPN Phenolic Cotton Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: BP11NPN is a phenolic canvas machining grade for structural and mechanical applications. It has better impact strength than phenolic paper grades.

Key Words: Cotton, Phenolic, Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
Moisture Absorption 3.50 %3.50 %Condition A; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Tensile Strength  66.9 MPa
@Thickness 3.17 mm
9700 psi
@Thickness 0.125 in
Condition A, Crosswise; ASTM D638
 82.7 MPa
@Thickness 3.17 mm
12000 psi
@Thickness 0.125 in
Condition A, Lengthwise; ASTM D638
Flexural Strength  117 MPa
@Thickness 1.57 mm
17000 psi
@Thickness 0.0620 in
Condition A, Crosswise; ASTM D790
 124 MPa
@Thickness 1.57 mm
18000 psi
@Thickness 0.0620 in
Condition A, Lengthwise; ASTM D790
Flexural Modulus  10.3 GPa
@Thickness 1.57 mm
1500 ksi
@Thickness 0.0620 in
Condition A, Crosswise; ASTM D790
 11.0 GPa
@Thickness 1.57 mm
1600 ksi
@Thickness 0.0620 in
Condition A, Lengthwise; ASTM D790
Compressive Strength 234 MPa
@Thickness 12.7 mm
34000 psi
@Thickness 0.500 in
Condition A, Flatwise; ASTM D695
Shear Strength 96.5 MPa
@Thickness 1.57 mm
14000 psi
@Thickness 0.0620 in
Condition A, Perpendicular; ASTM D732
Adhesive Bond Strength  15.9 MPa
@Thickness 12.7 mm
2300 psi
@Thickness 0.500 in
Condition D-48/50, Bonding Strength; ASTM D229
 17.2 MPa
@Thickness 12.7 mm
2500 psi
@Thickness 0.500 in
Condition A, Bonding Strength; ASTM D229
Izod Impact, Notched  1.44 J/cm
@Thickness 12.7 mm
2.70 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Crosswise; ASTM D256
 1.66 J/cm
@Thickness 12.7 mm
3.10 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Lengthwise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  5.91 kV/mm
@Thickness 1.57 mm
150 kV/in
@Thickness 0.0620 in
Condition D-48/50; ASTM D149
 15.7 kV/mm
@Thickness 1.57 mm
400 kV/in
@Thickness 0.0620 in
Condition A; ASTM D149
Dielectric Breakdown  5000 V
@Thickness 1.57 mm
5000 V
@Thickness 0.0620 in
Condition D-48/50; ASTM D149
 20000 V
@Thickness 1.57 mm
20000 V
@Thickness 0.0620 in
Condition A; ASTM D149
Arc Resistance 15 sec
@Thickness 3.17 mm
15 sec
@Thickness 0.125 in
Condition A; ASTM D495
Comparative Tracking Index 155 V
@Thickness 3.17 mm
155 V
@Thickness 0.125 in
ASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear  20.0 µm/m-°C
@Thickness 3.17 mm
11.1 µin/in-°F
@Thickness 0.125 in
X-axis; IPC-TM 650-2.4.24
 22.0 µm/m-°C
@Thickness 3.17 mm
12.2 µin/in-°F
@Thickness 0.125 in
Y-axis; IPC-TM 650-2.4.24
UL RTI, Electrical 115 °C239 °FUL Bulletin 746b
UL RTI, Mechanical without Impact 125 °C257 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
Condition A
 
Descriptive Properties
SubstrateCotton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNORPM226 / 280542

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.