MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ITW Irathane Futura® IRATHANE TX55 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: A single component roller, brush or spray applied inner coat adhesive developed for use with Irabond 9924 primer and Irathane and Aqualine system coats. UU55 is often recommended when repairing other polyurethane systems.

RECOMMENDED APPLICATIONS: Specifically designed for use with Irathane 155HS to enable an increased build to be achieved.

FEATURES: Increases viscosity of Irathane 155HS for increased build capability.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 149 °C>= 300 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 22.0 °C
12.0 Month
@Temperature 71.6 °F
In original unopened container in dry environment.
 
Descriptive Properties
ColorOpaque
Coverage4-10mL/10L KIT OF 155HS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWI9241 / 239750

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.