MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Karina 601-48/1-BY-IS-BZ Black PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Molded

Material Notes: Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.

Information provided by Karina Indústria e Comércio de Plásticos Ltda.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 - 1.38 g/cc1.25 - 1.38 g/ccASTM D 792
ASTM Color -1.02 - 0.58-1.02 - 0.58Color B, ME 12
 -0.860 - 0.74-0.860 - 0.74Color A, ME 12
 25.37 - 26.9725.37 - 26.97Color L, ME 12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  58 - 62
@Time 15.0 sec
58 - 62
@Time 0.00417 hour
ASTM D 2240
 58 - 62
@Time 15.0 sec
58 - 62
@Time 0.00417 hour
48HS; TL VW 676 PARTE 3.1.1/3.1.2
Tensile Strength >= 4.90 MPa>= 711 psiASTM D 638
Tensile Strength, Ultimate >= 4.90 MPa>= 711 psi80°C, 48 HS; TL VW 676 PARTE 3.4.2
Elongation at Break >= 200 %>= 200 %80°C, 48HS; TL VW 676 PARTE 3.5.2
 >= 200 %>= 200 %ASTM D 638
 
Descriptive Properties
ApplicationAutomotive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitriflex N-6420 NBR / PVC
Ensinger PVC Polyvinylchloride (PVC)
Denka VINYKON R2001 PVC, R grade for hard extrusion
Compuestos Dominicanos Polycom C-051065 PVC Compound
Colorite Polymers Flexchem 5051-02 Vinyl Compound

PKARIN9159 / 170815

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.