MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

General Industrial Polymers SBS – GP 87 Styrene/Butadiene/Styrene
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Features:
  • Oil-extended radial block copolymer
  • High strength and low viscosity
  • High tensile strength
  • Reprocess able
Typical Application:
  • Footwear compounding
  • Plastics modification

Information provided by General Industrail Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Volatiles 0.25 %0.25 %Typical; ASTM D5668
 <= 0.50 %<= 0.50 %Range; ASTM D5668
Melt Flow  12 g/10 min
@Load 5.00 kg,
Temperature 190 °C
12 g/10 min
@Load 11.0 lb,
Temperature 374 °F
Typical; ASTM D1238
 9.0 - 15 g/10 min
@Load 5.00 kg,
Temperature 190 °C
9.0 - 15 g/10 min
@Load 11.0 lb,
Temperature 374 °F
Range; ASTM D1238
Ash 0.20 %0.20 %Typical; ASTM D5667
 <= 1.0 %<= 1.0 %Range; ASTM D5667
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292Typical; ASTM D2240
 90 - 9490 - 94Range; ASTM D2240
 
Descriptive Properties
Content26-31%Oil, Range, ASTM D5774
 53-57%SM, Range, ASTM D5775
Content (%)28.5Oil, Typical, ASTM D5774
 55SM, Typical, ASTM D5775

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGENIND008 / 294797

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.