MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® 2730N Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Formolene® 2730N is a high impact copolymer of polypropylene designed and formulated for injection molded applications. It contains a combination of stabilizers and nucleators which provides an excellent balance of stiffness and cold temperature impact. Its range of physical and thermodynamic properties makes it an ideal choice for critical applications in the areas of automotive, appliances and lawn & garden. Formolene® 2730N meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact. This material is free of animal-derived content.

Information provided by Formosa Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 30 g/10 min
@Temperature 230 °C
30 g/10 min
@Temperature 446 °F
I2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.7 MPa2570 psi50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 896 MPa130000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched  1.23 J/cm
@Temperature -27.8 °C
2.30 ft-lb/in
@Temperature -18.0 °F
ASTM D256A
 5.87 J/cm
@Temperature 22.8 °C
11.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C198 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCPQ9022 / 239843

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.