MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite SI 9550 Silicone Molding Compound
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temperatures.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/ccASTM D792
Apparent Bulk Density 0.900 g/ccPowder; ASTM D1895
Water Absorption 0.090 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75ASTM D785
Tensile Strength 38.0 MPaASTM D638
Flexural Strength 65.0 MPaASTM D790
Flexural Modulus 13.0 GPaASTM D790
Compressive Strength 90.0 MPaASTM D695
Izod Impact, Notched 22.0 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 8.10 kV/mm
@Frequency 60 Hz
SS, wet; ASTM D149
 13.3 kV/mm
@Frequency 60 Hz
ST, wet; ASTM D149
Arc Resistance 240 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 282 °CPost Baked; ASTM D648A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUMIT196 / 194001

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.