MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teijin Panlite® ML-1105 Light Diffusion Grade Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Light diffusion grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: High Light diffusion. Uses: Automotive interior parts, lighting applications, LEDs, Lighting Diffusers. Appearance: Milky white. Forms: pellets. Processing Method: Injection Molding.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C,
Time 86400 sec
0.200 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 4.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.157 in
Teijin method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 4.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.157 in
Teijin method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.0 MPa8120 psiISO 527-2/50
Tensile Strength, Yield 61.0 MPa8850 psiISO 527-2/50
Elongation at Break >= 50 %>= 50 %ISO 527-2/50
Elongation at Yield 6.0 %6.0 %ISO 527-2/50
Tensile Modulus 2.40 GPa348 ksiISO 527-2/1
Flexural Strength 93.0 MPa13500 psi2.0 mm/min; ISO 178
Flexural Modulus 2.23 GPa323 ksi2.0 mm/min; ISO 178
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 4.00 J/cm²19.0 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 141 °C286 °Funannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °Funannealed; ISO 75-2/A
Vicat Softening Point 148 °C298 °FISO 306/B50
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 41 %
@Thickness 3.00 mm
41 %
@Thickness 0.118 in
ASTM D-1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® BL 6-2 820803 Polycarbonate
Covestro Makrofol® BL 6-2 820802 Polycarbonate
Teijin Panlite® ML-1103 Light Diffusion Grade Polycarbonate
Teijin Panlite® LN-2525ZA Polycarbonate
Teijin Panlite® ML-1102 Light Diffusion Grade Polycarbonate

PTEIH923 / 191615

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.