MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials Infino® NH-1015B PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Melt Flow 23.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
23.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 61.8 MPa8960 psi50 mm/min; ASTM D638
Flexural Strength 86.3 MPa12500 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.26 GPa327 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched 5.59 J/cm
@Thickness 3.17 mm
10.5 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C208 °FB/50; ISO 306
 100 °C212 °FB/120; ISO 306
UL RTI, Electrical 90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
V-0; UL 746B
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
V-0; UL 746B
UL RTI, Mechanical without Impact 90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
V-0; UL 746B
Flammability, UL94  V-1
@Thickness 1.20 mm
V-1
@Thickness 0.0472 in
 V-1
@Thickness 1.30 mm
V-1
@Thickness 0.0512 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 V-0
@Thickness 2.10 mm
V-0
@Thickness 0.0827 in
 V-0
@Thickness 2.50 mm
V-0
@Thickness 0.0984 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VB
@Thickness 2.50 mm
5VB
@Thickness 0.0984 in
 5VB
@Thickness 2.10 mm
5VB
@Thickness 0.0827 in
 5VB
@Thickness 2.50 mm
5VB
@Thickness 0.0984 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
Shrinkage, MD 0.00500 - 0.00700 %
@Thickness 3.20 mm
0.00500 - 0.00700 %
@Thickness 0.126 in
ASTM D955
Shrinkage, TD 0.00500 - 0.00700 %
@Thickness 3.20 mm
0.00500 - 0.00700 %
@Thickness 0.126 in
ASTM D955

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9507 / 325989

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.