MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Commercial Rolled Zinc (Zn-0.3Pb-0.03Cd; UNS Z21540), Cold-Rolled
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Used for soldered battery cans; photoengraving or lithography sheet. Not suited to long term load-bearing applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 170 MPaLongitudinal
 210 MPaTransverse
Elongation at Break 28 %Transverse
 45 %Longitudinal
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 - 40.0 °C
Transverse
 39.9 µm/m-°C
@Temperature 20.0 - 40.0 °C
Longitudinal
Specific Heat Capacity 0.395 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 108 W/m-K
Melting Point 419 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 105 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0010 %ASTM B 69
Cadmium, Cd 0.25 - 0.45 %ASTM B 69
Copper, Cu <= 0.0050 %ASTM B 69
Iron, Fe <= 0.0020 %ASTM B 69
Lead, Pb 0.25 - 0.50 %ASTM B 69
Tin, Sn <= 0.0010 %ASTM B 69
Zinc, Zn 99.041 - 99.5 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Hot-Rolled - Longitudinal Properties
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc ILZRO 16 (Zn-1.25Cu-0.2Ti-0.15Cr), Die Cast
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Hot-Rolled - Longitudinal Properties
Commercial Rolled Zinc (Zn-0.08Pb), Hot-Rolled - Longitudinal Properties

MZN761 / 106795

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.