MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HB5502B Blow Molding HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Hexene Copolymer

Applications: Injection blow molded pharmaceutical packaging

Formolene HB5502B is designed for applications requiring excellent stiffness and stress crack resistance properties. It may be used as a general-purpose blow molding resin or sheet extrusion thermoforming resin.

Produced using licensor formulation for HHM 5502BN. Licensor does not warrant or imply that this product meets their specifications for HHM 5502BN.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
Environmental Stress Crack Resistance 35 hourCondition B, F50; ASTM D1693
ESCR 100% Igepal® 45 hourCondition A, F50; ASTM D1693
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4000 psi2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 600 %2" (50mm) per min.; ASTM D638 Type IV
Flexural Modulus 200000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -180 °FASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® BG-15 PA6-GF15
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
SIDPEC EGYPTENE® HD 6070 UA HDPE Injection Molding
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin

PFPCPE13 / 38820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.