MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller TEC® 130 Ultimate Premixed Mortar
Categories: Polymer; Adhesive

Material Notes: Description: Ultimate Premixed Mortar is a premium ready to use adhesive, excellent for setting ceramic, porcelain, natural stone, quarry and mosaic tile on interior floors and walls. Recommended for wall and floor applications with tile up to 20" x 20". The lightweight composition offers easy troweling, non-slip wall performance, and non-slump floor performance. If mortar meeting ANSI A118.4 is required, TEC Ultimate Premixed Mortar may be used for glass tile up to 8” x 8".

Key Features and Benefits:

  • For tile and stone up to 20" x 20" on walls and floors
  • Lightweight—non-slip performance on walls, non-slump on floors.
  • Exceeds ANSI A136.1 Type I & II Specifications
  • Mold and mildew resistant
  • Fast drying
  • Creamy, easy to use formula

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 1.03 MPa149 psiType I Water Immersion
 3.42 MPa496 psi28 Day, Room Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL061 / 316852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.