Physical Properties | Metric | English | Comments |
---|
Density | 4.41 g/cc | 0.159 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Knoop | 1.41 | 1.41 |
Modulus of Elasticity | 21.5 GPa | 3120 ksi |
Poissons Ratio | 0.209 | 0.209 |
Fracture Toughness | 0.550 MPa-m½ | 0.501 ksi-in½ |
Shear Modulus | 8.89 GPa | 1290 ksi |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 12.1 µm/m-°C | 6.72 µin/in-°F |
Specific Heat Capacity | 0.330 J/g-°C | 0.0789 BTU/lb-°F |
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F |
Transformation Temperature, Tg | 368 °C | 694 °F |
|
Optical Properties | Metric | English | Comments |
---|
Refractive Index | 2.489 @Wavelength 12000 nm | 2.489 @Wavelength 12000 nm |
| 2.493 @Wavelength 11000 nm | 2.493 @Wavelength 11000 nm |
| 2.496 @Wavelength 10000 nm | 2.496 @Wavelength 10000 nm |
| 2.499 @Wavelength 9000 nm | 2.499 @Wavelength 9000 nm |
| 2.502 @Wavelength 8000 nm | 2.502 @Wavelength 8000 nm |
| 2.505 @Wavelength 7000 nm | 2.505 @Wavelength 7000 nm |
| 2.507 @Wavelength 6000 nm | 2.507 @Wavelength 6000 nm |
| 2.51 @Wavelength 5000 nm | 2.51 @Wavelength 5000 nm |
| 2.513 @Wavelength 4000 nm | 2.513 @Wavelength 4000 nm |
| 2.518 @Wavelength 3000 nm | 2.518 @Wavelength 3000 nm |
| 2.529 @Wavelength 2000 nm | 2.529 @Wavelength 2000 nm |
| 2.596 @Wavelength 1000 nm | 2.596 @Wavelength 1000 nm |
Transmission, Visible | 4.69 % @Wavelength 750 nm | 4.69 % @Wavelength 750 nm |
IR Transmittance | 3.98 % @Wavelength 12500 nm | 3.98 % @Wavelength 12500 nm |
| 6.47 % @Wavelength 13000 nm | 6.47 % @Wavelength 13000 nm |
| 17.86 % @Wavelength 12000 nm | 17.86 % @Wavelength 12000 nm |
| 24.58 % @Wavelength 13500 nm | 24.58 % @Wavelength 13500 nm |
| 32.98 % @Wavelength 800 nm | 32.98 % @Wavelength 800 nm |
| 43.43 % @Wavelength 14000 nm | 43.43 % @Wavelength 14000 nm |
| 49.53 % @Wavelength 11500 nm | 49.53 % @Wavelength 11500 nm |
| 49.76 % @Wavelength 850 nm | 49.76 % @Wavelength 850 nm |
| 56.57 % @Wavelength 900 nm | 56.57 % @Wavelength 900 nm |
| 59.16 % @Wavelength 950 nm | 59.16 % @Wavelength 950 nm |
| 60.43 % @Wavelength 1000 nm | 60.43 % @Wavelength 1000 nm |
| 62.51 % @Wavelength 1100 nm | 62.51 % @Wavelength 1100 nm |
| 63.64 % @Wavelength 11000 nm | 63.64 % @Wavelength 11000 nm |
| 63.79 % @Wavelength 1200 nm | 63.79 % @Wavelength 1200 nm |
| 64.06 % @Wavelength 8000 nm | 64.06 % @Wavelength 8000 nm |
| 64.5 % @Wavelength 1300 nm | 64.5 % @Wavelength 1300 nm |
| 64.9 % @Wavelength 1400 nm | 64.9 % @Wavelength 1400 nm |
| 65.08 % @Wavelength 1450 nm | 65.08 % @Wavelength 1450 nm |
| 65.42 % @Wavelength 1550 nm | 65.42 % @Wavelength 1550 nm |
| 65.99 % @Wavelength 1650 nm | 65.99 % @Wavelength 1650 nm |
| 66.09 % @Wavelength 1750 nm | 66.09 % @Wavelength 1750 nm |
| 66.2 % @Wavelength 1850 nm | 66.2 % @Wavelength 1850 nm |
| 66.33 % @Wavelength 1950 nm | 66.33 % @Wavelength 1950 nm |
| 66.4 % @Wavelength 4500 nm | 66.4 % @Wavelength 4500 nm |
| 66.52 % @Wavelength 2050 nm | 66.52 % @Wavelength 2050 nm |
| 66.55 % @Wavelength 2250 nm | 66.55 % @Wavelength 2250 nm |
| 66.56 % @Wavelength 2150 nm | 66.56 % @Wavelength 2150 nm |
| 66.68 % @Wavelength 2500 nm | 66.68 % @Wavelength 2500 nm |
| 66.74 % @Wavelength 2350 nm | 66.74 % @Wavelength 2350 nm |
| 66.76 % @Wavelength 2450 nm | 66.76 % @Wavelength 2450 nm |
| 66.94 % @Wavelength 5000 nm | 66.94 % @Wavelength 5000 nm |
| 67.13 % @Wavelength 10500 nm | 67.13 % @Wavelength 10500 nm |
| 67.29 % @Wavelength 3000 nm | 67.29 % @Wavelength 3000 nm |
| 67.51 % @Wavelength 3500 nm | 67.51 % @Wavelength 3500 nm |
| 67.75 % @Wavelength 8500 nm | 67.75 % @Wavelength 8500 nm |
| 67.76 % @Wavelength 9500 nm | 67.76 % @Wavelength 9500 nm |
| 67.78 % @Wavelength 9000 nm | 67.78 % @Wavelength 9000 nm |
| 67.92 % @Wavelength 4000 nm | 67.92 % @Wavelength 4000 nm |
| 67.97 % @Wavelength 10000 nm | 67.97 % @Wavelength 10000 nm |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.