MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GY-PEL-300 Polyolefinic Elastomer POE
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: GY-PEL-300 is olefinic elastomer mainly applied on compounding, film, sheeting and package application. It is a propylene based elastomer with high durability and mechanical properties.

Features:

  • durability and mechanical properties high compatibility
  • low seal initial temperature which can be well work with high seal strength for the layer from extruded processing method.
  • high chemical resistant ability
  • anti-aging ability
  • good adhesion
  • high toughness and flexibility
  • good elasticity
  • clarity
Applications:
  • blown Film
  • calendered Sheeting
  • cast Film
  • extruded Sheeting
  • injection Molding
  • PP/TPO Modification
  • compounding, film, sheeting and package
  • extruded processing method
  • PP, PE

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.873 g/cc0.0315 lb/in³
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3333
Tensile Strength at Break 17.1 MPa2480 psi
Tensile Stress  4.51 MPa
@Strain 300 %
654 psi
@Strain 300 %
 4.59 MPa
@Strain 100 %
666 psi
@Strain 100 %
Tensile Strength, Yield 5.22 MPa757 psi
Elongation at Break 1898 %1898 %
Elongation at Yield 48 %48 %
Tear Strength 62.3 kN/m355 plidie C
 
Descriptive Properties
AppearancePellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN712 / 267020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.