MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dow VORAFORCE™ TW 1150/TW 1100 Polyurethane for Composite Systems
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: The VORAFORCE™ TW series consists of formulated systems for filament winding applications. They exhibit excellent flow properties and fiber wetting due to low viscosities and long working times. This system combines good mechanical and electrical properties, as well as high temperature resistance and low moisture take-up.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 300 cP100 - 300 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 65.0 - 75.0 MPa9430 - 10900 psi
Flexural Strength 90.0 - 100 MPa13100 - 14500 psi
Fracture Toughness 1.60 - 1.80 MPa-m½1.46 - 1.64 ksi-in½
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 85.0 - 95.0 °C185 - 203 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
Pot Life 25.0 - 30.0 min25.0 - 30.0 min
 
Descriptive Properties
Mix Ratio105 phr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORAFORCE™ TW 103/TW 165/TC 3000 Epoxy for Composite Systems
Dow VORAFORCE™ TW 108/TW 120 Epoxy for Composite Systems
Dow VORAFORCE™ TW 108/TW 172 Epoxy for Composite Systems
Dow VORAFORCE™ TW 108/TW 158 Epoxy for Composite Systems
Dow VORAFORCE™ TW 103/TW 120 Epoxy for Composite Systems

PDOW0922 / 185333

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.