ALLEN® 2057MT is a general purpose ABS with medium impact and a matte gloss finish. ALLEN® 2057MT has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302). Suggested Application: - Medical Equipment Housings
- Food Equipment Trays & Housings
- Display
- Signs
Features: - Custom color matching
- Ease of processing
- Regrind compatible in future orders
- Matte gloss finish
Information provided by SEKISUI KYDEX, LLC. |