MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChenGuang CGF-268A PTFE Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Molecular formula: [CF2--CF2]n

CAS No. 9002-84-0

Description: CGF 268 is the virgin PTFE (polytetrafluoroethylene) powder for the applications to make rods, tubing etc. by paste extrusion. Its typical end products includes wire and cable insulating coating, linings, hoses, tubing, sleevings for use with heat, steam, hydraulic fluid, etc... Preferred for the extrusion processing with reduction ratios (i.e. RR) in the range 400 : 1 to 1500: 1. Typical products are extruded small tubing or rods, e.g. Ø 1.8 / 1.5 or Ø 0.9 / 0.5

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.16 - 2.20 g/cc2.16 - 2.20 g/cc
Bulk Density 0.375 - 0.575 g/cc0.0135 - 0.0208 lb/in³
Particle Size 400 - 600 µm400 - 600 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 24.0 MPa>= 3480 psi
Elongation at Break >= 300 %>= 300 %
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU036 / 255635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.