MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® NBX-0025 NF2001 PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 8.5 %ISO 62
Moisture Absorption at Equilibrium 2.5 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.016 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 83.0 MPa50mm/min; ISO 527
 83.0 MPa2 in/min; ASTM Test
Elongation at Break 25 %50mm/min, Nominal strain; ISO 527
 60 %2 in/min; ASTM Test
Elongation at Yield 5.0 %50mm/min; ISO 527
 5.0 %2 in/min; ASTM Test
Tensile Modulus 3000 MPa1mm/min; ISO 527
Flexural Strength 117 MPaASTM Test
Flexural Modulus 2800 MPaISO Data
 2900 MPaASTM Test
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 5.20 kJ/m²ISO Test
Charpy Impact Unnotched NBISO 179
 NB
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.570 J/cm²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °C10 K/min
 257 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75
 243 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CISO 75
 170 °CASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 101F NC010 PA66
Celanese Zytel® 101 NC010 PA66
Celanese Minlon® 10B40 NC010 PA66-MD40
BASF Ultramid® NBX-0025 NF2001 PA66 (Conditioned)
BASF Ultramid® A3W Q601 PA66 (Dry)

PBASF9383 / 85147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.