MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zenite® 7244 BK010 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Zenite® 7244 BK010 is a 40% glass/mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295°C, high flow and good flatness.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³ISO 1183
Filler Content 40 %40 %
Linear Mold Shrinkage, Flow 0.0010 cm/cm
@Thickness 2.00 mm
0.0010 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527
Elongation at Break 1.4 %1.4 %ISO 527
Tensile Modulus 14.0 GPa2030 ksiISO 527
Flexural Strength 180 MPa
@Temperature 23.0 °C
26100 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 11.3 GPa
@Temperature 23.0 °C
1640 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.9
@Thickness 2.00 mm,
Frequency 1e+10 Hz
3.9
@Thickness 0.0787 in,
Frequency 1e+10 Hz
Transverse; ASTM D2520 B
 4.1
@Thickness 2.00 mm,
Frequency 1e+9 Hz
4.1
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D2520 B
 4.2
@Thickness 2.00 mm,
Frequency 1e+10 Hz
4.2
@Thickness 0.0787 in,
Frequency 1e+10 Hz
ASTM D2520 B
 4.2
@Thickness 2.00 mm,
Frequency 2.00e+10 Hz
4.2
@Thickness 0.0787 in,
Frequency 2.00e+10 Hz
ASTM D2520 B
Dissipation Factor  0.0040
@Thickness 2.00 mm,
Frequency 1e+9 Hz
0.0040
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D2520 B
 0.0040
@Thickness 2.00 mm,
Frequency 1e+10 Hz
0.0040
@Thickness 0.0787 in,
Frequency 1e+10 Hz
Transverse; ASTM D2520 B
 0.0040
@Thickness 2.00 mm,
Frequency 1e+10 Hz
0.0040
@Thickness 0.0787 in,
Frequency 1e+10 Hz
ASTM D2520 B
 0.0040
@Thickness 2.00 mm,
Frequency 2.00e+10 Hz
0.0040
@Thickness 0.0787 in,
Frequency 2.00e+10 Hz
ASTM D2520 B
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
1.67 µin/in-°F
@Thickness 0.0787 in,
Temperature 320 - 500 °F
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
2.22 µin/in-°F
@Thickness 0.157 in,
Temperature 320 - 500 °F
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
2.78 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 23.0 °C
2.78 µin/in-°F
@Thickness 0.0787 in,
Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 260 °C
2.78 µin/in-°F
@Thickness 0.0787 in,
Temperature -40.0 - 500 °F
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 260 °C
3.33 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 500 °F
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
3.33 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
3.33 µin/in-°F
@Thickness 0.157 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
3.33 µin/in-°F
@Thickness 0.0787 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
 7.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
3.89 µin/in-°F
@Thickness 0.157 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow  32.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
17.8 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2; 2mm
 38.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
21.1 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2; 4mm
 42.0 µm/m-°C
@Temperature -40.0 - 260 °C
23.3 µin/in-°F
@Temperature -40.0 - 500 °F
ISO 11359-1/-2; 2mm
 50.0 µm/m-°C
@Temperature -40.0 - 260 °C
27.8 µin/in-°F
@Temperature -40.0 - 500 °F
ISO 11359-1/-2; 4mm
 35.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
19.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 41.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
22.8 µin/in-°F
@Thickness 0.157 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 45.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
25.0 µin/in-°F
@Thickness 0.0787 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
 48.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
26.7 µin/in-°F
@Thickness 0.0787 in,
Temperature 320 - 500 °F
ISO 11359-1/-2
 52.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
28.9 µin/in-°F
@Thickness 0.157 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
 58.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
32.2 µin/in-°F
@Thickness 0.157 in,
Temperature 320 - 500 °F
ISO 11359-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 295 °C563 °FISO 75-1/-2 1993/N2
UL RTI, Electrical 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
Flammability, UL94  V-0
@Thickness 0.350 mm
V-0
@Thickness 0.0138 in
IEC 60695-11-10
 V-0
@Thickness 0.350 mm
V-0
@Thickness 0.0138 in
UL94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 365 °C689 °FOptimum
 360 - 370 °C680 - 698 °F
Mold Temperature 80.0 °C176 °FOptimum
 40.0 - 150 °C104 - 302 °F
Drying Temperature 150 °C302 °F
Dry Time 3 hour3 hourDehumidified Dryer
Moisture Content <= 0.010 %<= 0.010 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FillerGlass/Mineral
FormsPellets
GenericLCP
Part Marking Code>LCP-(GF+MD)40<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass/Mineral Reinforced Resins
 Low Warp Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-(GF+MD)40ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese Zenite® 6635 BK010 LCP
Celanese Zenite® ZE55201 BK010 LCP

PDTA7788 / 89631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.