MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Micropol Microlink XL28 Crosslinkable Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, and temperature resistance. It is fully UV stabilized and available in colors for outdoor use in all climates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.943 g/ccASTM D1505
Environmental Stress Crack Resistance >= 1000 hourM F50; ASTM D1693
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 23.0 MPa50mm/min; ASTM D638
Elongation at Break 350 %ASTM D638
Flexural Modulus 0.750 GPaASTM D790
Impact 36
@Temperature -20.0 °C
J/mm, Micropol test based on ASTM D1790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 127 °CASTM D1525
Brittleness Temperature <= -120 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Micropol Microlink XL28/FR Black Crosslinkable Polyethylene
Micropol Isoplas P651 Crosslinkable Polyethylene
Micropol Isoplas P381 Crosslinkable Polyethylene
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene

PMICRO26 / 108456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.