MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAMID® eCO LX9039 BBM100 Nylon 12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® eCO LX9039 BBM100 is an unmodified, medium viscosity polyamide 12 without stabilizers and processing aids. It is usually used only in special cases where the absence of any additives is desirable or the presence of processing aids interferes. eCO stands for Evoniks aim to eliminate CO2 through use of renewable or circular feedstocks via mass-balance approach. VESTAMID® eCO LX9039 BBM100 is supplied as spherical granules, ready for processing in moisture-proof packaging. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering, Sports and Lifestyle
Sustainability: eCO
Delivery form: Pellets, Granules
Additives: Unfilled
Special Characteristics: Medium viscosity
Color: Natural color

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527
Tensile Strength 38.0 MPa5510 psiISO 527
Tensile Stress 31.0 MPa
@Strain 50.0 %
4500 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break 260 %260 %Nominal; ISO 527
Elongation at Yield 15.0 %15.0 %ISO 527
Tensile Modulus 1.00 GPa145 ksiISO 527
Flexural Strength 32.0 MPa4640 psiat conv. Deflection; ISO 178
 44.0 MPa6380 psiISO 178
Flexural Modulus 1.03 GPa149 ksiISO 178
Flexural Strain at Break 8.00 %8.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.20e+12 ohm-cm2.20e+12 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 62631-3-2
 
Descriptive Properties
Blue water consumption26.7 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential2.7 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 4.5 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)5.6 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7903 / 325035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.