Quenched and tempered high strength low alloy structural steel plates for welded, riveted or bolted construction. Intended primarily for use in welded bridges and buildings where savings in weight and notch toughness are important. Information provided by Bethlehem Steel Corporation Data published in 1997. Bethlehem Steel in no longer in business. |