MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aluminum 2011-T6
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Information provided by Alcoa and the references. General 2011 characteristics and uses: Good machinability, especially free-cutting qualities, good mechanical properties. Excellent surface finish capability. The T451 temper offers good deep drilling characteristics.

Uses: Adapters, carburetor parts, clock parts and gears, knobs, camera parts, meter shafts and gears, nozzles, pencil and pen parts, oil line filters, pipe stems and filters, radio parts, screwdriver caps, spindles, telephone parts, TV fittings, tripod fittings, machine parts, hose parts, pipe stems.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2011-T6; UNS A92011; QQ-A-225/3; NF A-U4Pb (France); DIN AlCuBiPb; BS FC1; AA2011-T6; Al2011-T6
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9797500 kg load with 10 mm ball
Hardness, Knoop 122122Converted from Brinell Hardness Value
Hardness, Rockwell A 40.440.4Converted from Brinell Hardness Value
Hardness, Rockwell B 6161Converted from Brinell Hardness Value
Hardness, Vickers 109109Converted from Brinell Hardness Value
Tensile Strength, Ultimate 395 MPa57300 psi
Tensile Strength, Yield 270 MPa39200 psi
Elongation at Break 17 %
@Thickness 1.60 mm
17 %
@Thickness 0.0630 in
In 5 cm
Modulus of Elasticity 70.0 GPa10200 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33
Fatigue Strength 125 MPa
@# of Cycles 5.00e+8
18100 psi
@# of Cycles 5.00e+8
Shear Modulus 26.0 GPa3770 ksi
Shear Strength 235 MPa34100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.4 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.9 µin/in-°F
@Temperature -58.0 - 68.0 °F
 22.9 µm/m-°C
@Temperature 20.0 - 100 °C
12.7 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.0 µm/m-°C
@Temperature 20.0 - 200 °C
13.3 µin/in-°F
@Temperature 68.0 - 392 °F
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 170 W/m-K1180 BTU-in/hr-ft²-°FEstimated from trends in similar alloys.
Melting Point 540.6 - 643 °C1005 - 1190 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting can be eliminated by homogenization.
Solidus 540.6 °C1005 °FAA; Typical
Liquidus 643 °C1190 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 524 °C975 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.2 - 94.6 %91.2 - 94.6 %As remainder
Bismuth, Bi 0.20 - 0.60 %0.20 - 0.60 %
Copper, Cu 5.0 - 6.0 %5.0 - 6.0 %
Iron, Fe <= 0.70 %<= 0.70 %
Lead, Pb 0.20 - 0.60 %0.20 - 0.60 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Zinc, Zn <= 0.30 %<= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2011-T3
Aluminum 2011-T4
Aluminum 2011-T8
Aluminum 6061-T6; 6061-T651
Aluminum 2024-T6

MA2011T6 / 8835

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.