MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Meropa® 1500
Categories: Fluid; Lubricant

Material Notes: Texaco Meropa oils deliver value through:
  • Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubrication. High oxidation stability limits in-service viscosity increases, which lead to energy losses.
  • Extended equipment life — Extremely effective EP system forms a protective film in areas of metalto-metal contact, minimizing wear rates and maintaining efficient transfer of power. Good water separation and effective rust inhibitors protect surfaces against rust and corrosion. High thermal stability additive system reduces the formation of high temperature compounds which can be corrosive to bearing materials. The effective corrosion inhibitor provides additional protection for metal components
  • Long oil life — Effective oxidation inhibitors and copper passivator minimize oil oxidation, limiting viscosity increase and extending oil drain intervals.

Texaco Meropa oils are high performance, multipurpose gear lubricants designed for industrial gear lubrication services where loads and shock loadings are high.

When used in misting systems, Texaco Meropa provides excellent oxidation stability to prevent oil mist deposits. They will form a high volume of mist droplets for transmission to the point of application. Texaco Meropa oils have minimal stray mist (fog).

Texaco Meropa oils are recommended for:

  • All industrial enclosed gearing and wherever an AGMA extreme pressure lubricant is specified
  • All mist oil application systems
  • General industrial plant lubrication where the performance properties of this type of lubricant are required.

Texaco Meropa meet the requirements of:
  • U.S. Steel 224 (ISO 68, 100, 150, 220, 320, 460, 680)
  • AGMA 9005 (ISO 68, 100, 150, 220, 320, 460, 680, 1000, 1500)
  • Cincinnati Machine P-63 (ISO 68), P-76 (ISO 100), P-77 (ISO 150), P-74 (ISO 220), P-59 (ISO 320), P-35 (ISO 460), P-78 (ISO 1000)

Texaco Meropa oils (ISO 68, 100, 150, 220, 320, 460) are suitable for use in Bijur oil application equipment.

For customers wishing to extend drain intervals and further reduce gear wear, and where water contamination is minimal, Texaco Meropa oils are recommended. Texaco Meropa oils can be used in industrial applications where overloading, severe operating conditions, high lubricant operating temperatures, or other problems are encountered. Texaco Meropa oils have been shown to reduce operating temperatures, power consumption/energy requirements, and failure rates in industrial operating environments.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222344; MSDS Number: 8642

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 25.7 °
Viscosity Measurement 114Viscosity Index
Saybolt Viscosity at 100°F 7699 SUS
Saybolt Viscosity at 210°F 359 SUS
Kinematic Viscosity at 40°C (104°F) 1425 cSt
Kinematic Viscosity at 100°C (212°F) 74 cSt
 
Mechanical PropertiesOriginal ValueComments
Timken Test 65.0 lbOK Load
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 260 °C
 
Descriptive Properties
AGMA Grade9 EP
FZG Pass Stagemin 12ASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants PG-44A Grease
Nye Lubricants PG-3S Grease
Nye Lubricants PG-2S Grease
Nye Lubricants PG-1S Grease
Nye Lubricants 876M-MS FG) Grease

WTEXA106 / 76985

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.