MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Krytox® 1514 Vacuum Pump Fluid
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox® VPF fluids are inert and nonreactive to all elastomers, plastics, and metals. A version with antirust protection, 1514XP, is also available.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.55 g/cc
@Temperature 200 °C
0.0560 lb/in³
@Temperature 392 °F
 1.74 g/cc
@Temperature 100 °C
0.0629 lb/in³
@Temperature 212 °F
 1.83 g/cc
@Temperature 50.0 °C
0.0661 lb/in³
@Temperature 122 °F
 1.89 g/cc
@Temperature 20.0 °C
0.0683 lb/in³
@Temperature 68.0 °F
Kinematic Viscosity  1.7 cSt
@Temperature 200 °C
1.7 cSt
@Temperature 392 °F
ASTM D445
 142 cSt
@Temperature 20.0 °C
142 cSt
@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 32 cSt32 cSt50°C; ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.2 cSt7.2 cStASTM D445
Molecular Weight 3500 g/mol3500 g/molNMR
Vapor Pressure Test 2.00e-7 torr2.00e-7 torr20°C; Knudsen
 0.00000300 torr0.00000300 torr50°C; Knudsen
 0.000100 torr0.000100 torr100°C; Knudsen
 0.0100 torr0.0100 torr200°C; Knudsen
Evaporation Loss 1.0 %1.0 %Volatility; 22 hr; 149°C; ASTM D792
 3.0 %3.0 %Volatility; 22 hr; 204°C; ASTM D792
 1.9 %
@Temperature 121 °C,
Time 79200 sec
1.9 %
@Temperature 250 °F,
Time 22.0 hour
Volatility; ASTM D2595
Surface Tension 18 dynes/cm18 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 29.3 J/g
@Temperature 150 - 250 °C
12.6 BTU/lb
@Temperature 302 - 482 °F
Knudsen
Distillation Temperature 200 - 280 °C392 - 536 °FDistillation Range at 0.4 torr
Pour Point -54.0 °C-65.2 °FASTM D97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® 1506 Vacuum Pump Fluid
Chemours Krytox® 101 GPL Oil
Chemours Krytox® 100 GPL Oil
Chemours Krytox® 1645 Vacuum Service Fluid
Chemours Krytox® 16256 Vacuum Pump Fluid

WDUPK13 / 75373

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.