MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Hyflon® PFA P455X Perfluoroalkoxy  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic to 250-260°C (482-500°F) and are the material of choice in applications such as linings in the Chemical Process Industry, Specialty Cables, Semiconductor Industry, Aerospace, and other challenging industries. This product is a low molecular weight, high melt flow rate resin designed for cable extrusion and injection molding. Hyflon® PFA P455X is an ASTM D3307-Type IV resin.

Availability:

  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
Features:
  • Flame Retardant
  • High Heat Resistance
  • Low Flow
  • Semi Crystalline
Uses:
  • Aerospace Applications
  • Cable Jacketing
  • Liners
  • Piping
  • Semiconductor Molding Compounds
  • Tubing
Forms: Pellets

Processing Method: Extrusion

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.13 - 2.18 g/cc0.0770 - 0.0788 lb/in³ASTM D792
Melt Flow 22 - 28 g/10 min
@Load 5.00 kg,
Temperature 372 °C
22 - 28 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60ASTM D2240
Tensile Strength at Break >= 22.0 MPa>= 3190 psiASTM D1708
Elongation at Break >= 280 %>= 280 %ASTM D1708
Tensile Modulus 0.500 - 0.600 GPa72.5 - 87.0 ksiASTM D1708
Charpy Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant  2.1
@Frequency 50 Hz
2.1
@Frequency 50 Hz
ASTM D150
 2.1
@Frequency 100000 Hz
2.1
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 35.0 - 40.0 kV/mm889 - 1020 kV/inASTM D149
Dissipation Factor  <= 0.00050
@Frequency 50 Hz
<= 0.00050
@Frequency 50 Hz
ASTM D150
 <= 0.00050
@Frequency 100000 Hz
<= 0.00050
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 25.0 - 35.0 J/g10.8 - 15.1 BTU/lbASTM D4591
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C66.7 - 111 µin/in-°FASTM D696
Specific Heat Capacity 0.900 - 1.10 J/g-°C0.215 - 0.263 BTU/lb-°FASTM D1269
Thermal Conductivity 0.200 W/m-K
@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 300 - 310 °C572 - 590 °FASTM D3307
Crystallization Temperature 279 - 289 °C534 - 552 °FASTM D4591
Maximum Service Temperature, Air 260 °C500 °F
Flammability, UL94 V-0V-0
Oxygen Index 95 %95 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kazanorgsintez Diphenyloxide, Technical

PSOLVAY526 / 218254

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.