MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

LNP NORYL® MX5759 Polyphenylene Ether + Polystyrene, 20% Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: Will be commercialized as SGFN2HF.

  • Features: High flow
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 110 MPa16000 psiType I, 5 mm/min; ASTM D638
Flexural Yield Strength 141 MPa20500 psi(102 mm Span) 3mm/min; ASTM D790
Flexural Modulus 5.86 GPa850 ksi(102 mm Span) 3mm/min; ASTM D790
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inASTM D256
Izod Impact, Unnotched 4.54 J/cm8.51 ft-lb/inASTM D256
Falling Dart Impact 1.07 J0.789 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance <= 60 sec<= 60 sec(Tungsten Electrode, 3.18 mm) (PLC = 7); ASTM D495
Comparative Tracking Index 400 - 599 V
@Thickness 3.18 mm
400 - 599 V
@Thickness 0.125 in
PLC = 1; UL 746
Hot Wire Ignition, HWI >= 120 sec
@Thickness 3.18 mm
>= 120 sec
@Thickness 0.125 in
PLC = 0; UL 746
High Amp Arc Ignition, HAI 60 - 119 arcs
@Thickness 3.18 mm
60 - 119 arcs
@Thickness 0.125 in
PLC = 1; UL 746
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
@Thickness 3.18 mm
>= 5.91 in/min
@Thickness 0.125 in
PLC = 4; UL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 3.18 mm
270 °F
@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical 110 °C230 °FUL 746
UL RTI, Mechanical with Impact 105 °C221 °FUL 746
UL RTI, Mechanical without Impact 110 °C230 °FUL 746
Flammability, UL94  V-1
@Thickness 1.47 mm
V-1
@Thickness 0.0579 in
 V-0
@Thickness 5.99 mm
V-0
@Thickness 0.236 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 299 °C480 - 570 °F
Middle Barrel Temperature 260 - 304 °C500 - 579 °F
Front Barrel Temperature 271 - 310 °C520 - 590 °F
Nozzle Temperature 282 - 310 °C540 - 590 °F
Melt Temperature 282 - 310 °C540 - 590 °F
Mold Temperature 76.7 - 104 °C170 - 219 °F
Drying Temperature 104 - 110 °C219 - 230 °F
Dry Time 3 - 8 hour3 - 8 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Shot Size 30 - 70 %30 - 70 %Suggested
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP NORYL® PX2926 Polyphenylene Ether + Polystyrene, Filled

PZLNP1259 / 51341

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.