MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KLJ Group KANATOL 1000 L Plasticizer
Categories: Fluid

Material Notes: Properties: K-1000L is almost colourless and odorless oily liquid, free of foreign materials. K-1000L is a primary monomeric plasticizer with Linear character for Vinyl homo and Copolymers resins .It is, slightly insoluble in water but soluble in alcohols, hexane etc. and is miscible and compatible with all the monomeric plasticizers of PVC compounding.

Application: K-1000L is having lower volatile character than DIDP and suggested for the applications, where High stability is required at high and low temperature along with good electrical properties.

Chemical Name: 1,2 Benzenedicarboxylic acid, di Carpic ester

Molecular Formula: C 26 H46 O4

Molecular Structure: C6 H4 [COO(CH2)9]2

CAS Number: 84-77-5

EINECS NO.: 201-561-6

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.956 - 0.962 g/cc
@Temperature 27.0 °C
0.956 - 0.962 g/cc
@Temperature 80.6 °F
ASTM D1045-08
Viscosity 44 - 50 cP44 - 50 cPKLJ TM-P-13-97
Molecular Weight 446.66 g/mol446.66 g/mol
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.13e+10 - 2.13e+11 ohm-cm1.13e+10 - 2.13e+11 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Boiling Point 261 °C
@Pressure 0.000667 MPa
502 °F
@Pressure 0.0967 psi
IS 5298-05
Flash Point >= 230 °C>= 446 °FCOC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.483 - 1.489
@Temperature 27.0 °C
1.483 - 1.489
@Temperature 80.6 °F
ASTM D1045-08
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM E203-08
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.03%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.01%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<20Hazen, ASTM D1045-08
Content<0.1%Residual/Free Alcohol, KLJ TM-P-12-98
 >99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 248-254 mg KOH/gmEster Value, ASTM D1045-08
Volatile Loss<0.1%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ229 / 284250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.