MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carbon-Core CarbonFoam PU 6 R PU
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Standard sheet size is 48” X96”
All CarbonFoam PU products can be supplied in customer specified CNC cut kit form.
Closed cell content up to 95%
Freeze and thaw cycle tested.
Anti-static additives available for specific applications.
Low-abrasion additives available for machining applications.
Fire - retardant additives available.

Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.070 %0.070 %ASTM C272
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.655 MPa95.0 psiASTM D1623
Tensile Modulus 0.0165 GPa2.40 ksiASTM D1623
Flexural Strength 1.10 MPa160 psiASTM D790
Compressive Strength 0.896 MPa130 psiPerpendicular to ruse-width; ASTM D1621
 0.896 MPa130 psiPerpendicular to rise-length; ASTM D1621
 0.965 MPa140 psiparallel to rise-thickness; ASTM D1621
Compressive Modulus 0.0193 GPa2.80 ksiPerpendicular to ruse-width; ASTM D1621
 0.0193 GPa2.80 ksiPerpendicular to rise-length; ASTM D1621
 0.0214 GPa3.10 ksiASTM D1621
Shear Modulus 0.00552 GPa0.800 ksiASTM C273
Shear Strength 0.552 MPa80.0 psiASTM C273
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.31.3
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0288 W/m-K0.200 BTU-in/hr-ft²-°FK-Factor
Insulation R Value 5.35.3
 
Descriptive Properties
Buoyancy54.4 lb/ft3
Closed Cell Rate0.95
Dimensional Stability-297-300°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M K37 Glass Bubbles
3M K25 Glass Bubbles
3M S38HS Glass Bubbles
3M S38 Glass Bubbles
3M S35 Glass Bubbles

PCARBC007 / 190826

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.