Description: Condensation crosslinking silicone casting compound for pad printing, shore A 18 Key Features - 100:3 mix ratio
- Low viscosity
- Suited printing pad manufacture
- Shore A 18
Application: PAD printingCured Product: Standard climate DIN 50 014 - 23/50-2. Vulcanizate tested after 7 days at room temperature Information provided by CHT Group |