  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
 9898heat aged 70 hours at 300ºF
 9898heat aged one week at 300ºF
Tensile Strength 9.79 MPa1420 psiheat aged one week at 300ºF
 10.0 MPa1450 psiheat aged 70 hours at 300ºF
 15.9 MPa2310 psi
Elongation at Break 50 %50 %heat aged 70 hours at 300ºF
 60 %60 %heat aged one week at 300ºF
 200 %200 %
100% Modulus 11.4 MPa
@Strain 100 %
1660 psi
@Strain 100 %
200% Modulus 15.9 MPa
@Strain 200 %
2310 psi
@Strain 200 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 152 °C
0.500 hour
@Temperature 305 °F
 
Descriptive Properties
Formulation as Tested0.25Stearic Acid
 100Millathane 5004
 6Di-Cup 40C
 80N330 (HAF) Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMILL356 / 87400

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.