MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes EF529AA an excellent choice for profile extrusions, molding, and foaming applications requiring medium VA content.

    Application/Uses
  • Flexible packaging films
  • Peelable seals, adhesive layers
  • Injection and blow molding
  • Hot melt adhesives and blends
  • Profile extrusions, tubing, wire & cable

This resin grade complies with 21 CFR, section 177.1350.

Key Words: Excellent optics and low heat seal initiation. 18.5% EVA.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccD1505
Vinyl Acetate Content 18.5 %
Thickness 31.75 micronsThickness Tested
Melt Flow 2.5 g/10 minD1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 600 %D882
Film Elongation at Break, TD 800 %D882
Dart Drop 232 g/milD1709
Dart Drop Test 290 gD1709
Film Tensile Strength at Break, MD 24.8 MPaD638
Film Tensile Strength at Break, TD 24.1 MPaD638
1% Secant Modulus, MD 42.1 MPaD882
1% Secant Modulus, TD 50.3 MPaD882
 
Thermal PropertiesOriginal ValueComments
Melting Point 85.0 °CDSC Peak; D33418
Vicat Softening Point 67.0 °CD1525
 
Optical PropertiesOriginal ValueComments
Haze 3.6 %D1003
Gloss 82 %at 45°; D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 177 °CBlown Film
 <= 204 °CCast Film
Blow-up Ratio (BUR) 2.5As tested
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem CN8092 EVA Molding Copolymer
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer
Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer
Bamberger Polymers Bapolene® EVA-1122 Ethylene Vinyl Acetate (EVA)

PBP1129e / 146113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.