MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT HANSA CARE 6730 ECO PDMS emulsions
Categories: Other Engineering Material

Material Notes: Description: PDMS emulsions are an universal ingredient for formulating products for home and car care applications. The PDMS emulsions are easy to use and have a good dilution stability. The products can be used to improve gloss, smoothness, softness and water repellency.

Key Features

  • Enhances gloss
  • Increases color depth and has color restoring properties
  • Smoothness and leveling
  • Water repellency
Key Applications
  • Leather and Furniture Care
  • Car Care
  • Tyre and Vinyl Care
  • Polishes
Application: HANSA CARE 6730 ECO can be applied as care component for aqueous care formulations.

Addition Rates
Dosage 1: 1.0 – 30.0% in total formulations

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 60 %60 %
pH 6.5 - 8.06.5 - 8.010% solution
Viscosity Measure 12500 cSt12500 cStBase Fluid
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceWhite liquid
ChemistryPDMS emulsion
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL276 / 314759

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.